600℃ LY-DSC300 Differential Scanning Calorimeter DSC

Dongguan Liyi Environmental Technology Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

600℃ LY-DSC300 Differential Scanning Calorimeter DSC

  • 1
  • 2
  • 3

Brand Name : LIYI

Model Number : LY-DSC300

Place of Origin : China

MOQ : 1 Set

Packaging Details : Wooden box

Contact Now

►Product introduction:

LY-DSC300 is one of the most accurate DSC series products launched by the company. The sensor is made of imported material E-pair, which has high accuracy, high sensitivity and good repeatability. The signal acquisition circuit has shielding protection, strong anti-interference, and extremely high baseline stability and repeatability.

LY-DSC300 differential scanning calorimeter can be used to test glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature, product stability, oxidation induction period, etc. It is competent in the research of pipes, polymers, chemicals, food, medical treatment and many other fields, and its products serve universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.

►Technical parameter:

1. Temperature range :Room temperature~600℃

2. Temperature resolution: 0.001℃

3. Temperature fluctuation:±0.001℃

4. Temperature repeatability:±0.01℃

5. Heating rate: 0.1~100℃/min

6. Incubation time:Program setting≤300min

7. Temperature Control:Heating up, constant temperature, cooling down(Full automatic program control)

8. DSC Range: 0~±600mW

9. DSC Resolution: 0.01uW

10. DSC Sensitivity: 0.001mW

11. Working Power Supply: AC220V/50Hz Or customized

12. Atmosphere Control Gas:Nitrogen, Oxygen(Program setting/automatic switching)

13. Gas Flow:0-200mL/min

14. Gas Pressure:0.2MPa

15. Display Mode: 24bit color,7-inch LCD touch screen display

16. Data Interface:Standard USB interface

17. Parameter standard: Equipped with reference materials (indium, tin),The user can correct the temperature by himself

18. The instrument has multiple sets of thermocouples,Temperature of a group of measured samples,One group to measure furnace temperature,One group measures the internal ambient temperature

19. Cooling device:Air cooling device(Optional semiconductor<-40~550℃>,Liquid nitrogen refrigeration<-150~550℃>)

►Technical characteristics:

  • Industrial 7-inch touch screen with rich information.
  • New furnace structure, better baseline and higher precision. Heating by indirect conduction, high uniformity and stability, reduced pulse radiation, better than traditional heating mode.
  • USB communication interface, with strong universality, reliable communication without interruption, and support for self recovery connection function.
  • Automatic switching of two atmospheric flows, fast switching speed and short stabilization time. At the same time increase one way protective gas input.
  • The software is simple and easy to operate.
  • Ultra high sensitivity,accuracy, 0.001mw,0.001℃
  • Excellent technical indicators,Superior performance,High cost performance,Widely used.

600℃ LY-DSC300 Differential Scanning Calorimeter DSC


Product Tags:

600℃ Differential Scanning Calorimeter

      
Quality 600℃ LY-DSC300 Differential Scanning Calorimeter DSC for sale

600℃ LY-DSC300 Differential Scanning Calorimeter DSC Images